the object of the application is the way the manufacture of application of thermal blankets foam polystyrene, in which the raw material in the form of granules of polystyrene is subjected to preheating temperature from 35 to 55u00b0c in time from 30 to 90 seconds, with pre heated process it takes place in u015blimakowym dispenser using heat energy recovered in the process of the foam.then the pre heated raw material is then foamed foam process, the raw material is subjected to the ageing process in constant temperature from 30 to 120 degrees in the time from 4 to 8 hours, with the process of ageing is carried out using the heat energy recovered in the process ie formation in block, then the raw material is subjected to wysezonowany process moulding in blockthe raw material is added from 1 to 3% by weight ekspandowanego glass granules size grains from 0.04 to 0.125 mm, and in the final stage of forming in the block of material is subjected to the action of the vacuum, air, and then pressure air or inert gas in the range from 0 3 to 0,6 bar at a time from 30 to 90 seconds,and then a raw material is subjected to ageing process block in temperature from 10 to 105 in a time from 36 to 60 hours, preferably 48. termoizolacyjny element of foamed polystyrene, in which the level of the deviation density in unit weight is + / - 0.1 0.1 kg / m3, containing from 1 to 3% by weight ekspandowanego glass granules size grains from 0.04 to 0.125 mm.
机译:本申请的目的是制造热毯泡沫聚苯乙烯的方法,其中将聚苯乙烯颗粒形式的原料在30至90秒的时间内经受35至55的预热温度,预热过程是在泡沫分配器中利用在泡沫过程中回收的热能进行的。然后将预热的原材料进行发泡泡沫过程,将原材料在30至120度的恒定温度下进行时效处理在4到8个小时的时间内,使用在过程中回收的热能(即成块地进行)进行时效过程,然后对原材料进行wysezonowany成型加工,然后将原材料从1-3添加重量百分比ekspandowanego玻璃颗粒的晶粒尺寸为0.04至0.125 mm,在成型的最后阶段,材料块要经受真空,空气,确保空气或惰性气体在30到90秒的时间内在0 3到0.6 bar范围内,然后在36到60个小时的时间内在10到105的温度下对原料进行时效处理,最好是48.泡沫聚苯乙烯的termoizolacyjny元素,其中单位重量的偏差密度为+0.1-0.1 kg kg / m3,包含1-3%重量的ekspandowanego玻璃颗粒,粒度为0.04至0.125毫米

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号