Method for obtaining nanocrystalline iron oxide using the solvothermal method

机译:溶剂热法制备纳米晶氧化铁的方法

摘要

method for nanokrystalicznego iron oxide using the method solwotermalnej, characterised by the fact that the soluble iron salt in polyethylene glycol added sodium acetate, placed so obtained, a clear solution in microwave reactor and is syntez r in the presence of solvent niewodnego of polyethylene glycol.in the temperature range of 130u00b0c to 174u00b0c, by microwaves in the 25 - 45%., is a suspension of nanoparticles of iron oxide and iron oxide nanoparticles are separated from the solution by decantation using permanent magnet and repeated przepu0142ukaniu alcohol and water.
机译:一种使用solwotermalnej方法的纳米晶体氧化铁的方法,其特征在于在聚乙二醇中的可溶性铁盐中加入乙酸钠,如此放置,在微波反应器中得到澄清溶液,并且在聚乙二醇新溶剂的存在下合成。在温度为130 u00b0c至174 u00b0c的范围内,通过25%-45%的微波,形成了氧化铁纳米颗粒的悬浮液,并且使用永磁体通过倾析和重复的przep从溶液中分离出氧化铁纳米颗粒酒精和水。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号