the subject of the invention is a way of flexible antennas operating in the ghz based on reduced graphene oxide of any shape on a flexible substrate.implementation of flexible antennas operating in the ghz based on reduced graphene oxide of the invention uses the method of printing inkjet printing layers of graphene oxide.using the printer inkjet guided computer developed template printing on pet substrate by ink is applied.it contains flakes of graphene oxide suspended in ethylene glycol propylene glycol with a density of 1 - 1.3 g / cm3, flow index 0.80 - 0,95, controlling 12.0 - 12.3 mpas and surface tension - 35.0 30.0 mj / s2.the layer of ink is applied jednoprzebiegowo in volume 1 - 1.2 ml / cm2. subsequently, a printout is dried at 60 - 70u00b0c for 30 - 40 minutes.in the next stage of drying print is given on the table working laser uv remote computer according to the prepared template and subjected to reduction, whereby the power beam is 1 - 2,the outbreak of 4.5 - 5 mm, and the velocity of 100 - 120 cm / s. so prepared antenna is secured uv varnish.
机译:本发明的主题是一种基于在柔性基板上基于任何形状的还原氧化石墨烯在ghz中工作的柔性天线的方法。基于本发明的基于基于还原氧化石墨烯的ghz中工作的柔性天线的实现使用印刷喷墨的方法氧化石墨烯的印刷层。使用打印机喷墨指导的计算机开发的模板,在宠物基材上通过油墨进行印刷。它包含悬浮在乙二醇丙二醇中的氧化石墨烯薄片,密度为1-1.3 g / cm3,流动指数为0.80 -0.95,控制12.0-12.3 mpas和表面张力-35.0 30.0 mj / s2。在jednoprzebiegowo上以1-1.2 ml / cm 2的体积施加墨水层。随后,将打印输出在60-70 u00b0c干燥30-40分钟。在干燥的下一阶段,根据准备好的模板,在台式激光uv远程计算机上进行打印,并进行还原,从而将功率束1-2,爆发4.5-5 mm,速度100-120 cm / s。因此,准备好的天线要经过紫外线清漆处理。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号