the object of the application is a synthesis zeolite from the ashes resulting from the incineration and co incineration of biomass of phosphatase or activation under conditions of high pressure charakteryzuju0105cy that to the pressure reactor is composition of fly ash containing in its chemical composition components of sio2 oxide, 20 to 60% by weight of al2o3, 2,1 - 13% by weight, which composition contains the ashes resulting from the incineration and co incineration or biomass, the following factor alkaline in quantities of from 1 to 20 ml per 1 g of fly ash.optional introduces modifying factors, the resulting mixture is mixed, initially raises the pressure in the reaction to the level of 0,1 - 0.6 mpa.maintains the reactionary in this state for the period from 2 to 10 minutes.then the system is heated to temperature above 70u00b0c reactionary at constant speed while increasing the pressure in the reaction system to a level above 1 mpa, preferably to a level 1.1 - 1.8 mpa and maintains a reactionary in this state for the period from 1 to 6 hours, then the reactionary cools at a constant speed, removes excess alkaline reaction system factor.and the product obtained is washed with water at elevated temperature, washing to a ph value in the water rinsing and then drying.with the compositions of volatile synthesis zeolite using materials such as fly ash from biomass burning in boilers and fluidalnych slatted ash fly;ne derived from co incineration of biomass boilers slatted and fluidalnych with coal, coal to biomass proportions from 100: 1 to 1: 100.the mixture formed by mixing the ashes to ashes volatile incineration or co incineration ashes from combustion of biomass and coal in appropriate proportions.
机译:本申请的目的是由磷酸酶的生物质的焚化和共焚化或在高压下的灰化合成灰分的合成沸石。氧化硅,重量百分比为20至60%的氧化铝,重量百分比为2,1至13%,该成分包含焚烧和共焚化产生的灰烬或生物质,以下碱性成分每1毫升为20毫升每克粉煤灰。可选地引入改性因子,将所得混合物混合,首先将反应压力升高至0.1-0.6 mpa的水平,使反应器在此状态下保持2至10分钟。将系统以恒定速度加热到高于70℃的温度,同时将反应系统中的压力增加到1 mpa以上,最好增加到1.1-1.8 mpa,在此状态下保持反应1到6个小时,然后以恒定速度冷却反应,除去过量的碱性反应体系因子,然后将所得产物在高温下用水洗涤,将其洗涤至ph值使用挥发性合成沸石的成分,使用锅炉中燃烧生物质的粉煤灰和流化板条飞灰等材料制成的挥发性合成沸石;由板条化和流化的生物质锅炉与煤,煤与生物质的比例为100的共焚化制得的1:1:1:100。以适当的比例将灰分混合成灰分,以燃烧生物质和煤炭燃烧而产生的挥发性焚烧灰或联合焚烧灰。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号