首页> 外国专利> A PROCESS FOR THE PRODUCTION OF POTASSIUM SULPHATE AND MAGNESIUM SULPHATE FROM CARNALLITE AND SODIUM SULPHATE

A PROCESS FOR THE PRODUCTION OF POTASSIUM SULPHATE AND MAGNESIUM SULPHATE FROM CARNALLITE AND SODIUM SULPHATE

机译:由钠钙石和硫酸钠生产硫酸钾和硫酸镁的工艺。

摘要

According to some embodiments there is provided a process for the recovery of SOP from Sulphate bearing mineral and Carnallite or Sylvenite, comprising: Dissolving Carnallite in water to obtain Sylvenite and high Magnesium Chloride brine; Adding Sodium Sulphate to said Carnallite to produce mixture of KainteLeonite, KCl and NaCl precipitant and brine containing Mg Cl2, KCl, NaCl; Separating the NaCl from the mixture; Obtaining a precipitant mixture of Leonite with KCl; Filtering said Leonite and washing with water to yield pure mixture of Leonite with KCl; Adding KCl to the Leonite with the KCl; and Decompose said Leonite with the KCl to SOP.
机译:根据一些实施方案,提供了一种用于从含硫酸盐的矿物和卡纳利特或方钠石中回收SOP的方法,该方法包括:将卡纳利特溶解在水中以获得方钠石和高氯化镁盐水;将硫酸钠加到所说的Calnallite中,以产生Kainte Leonite,KCl和NaCl沉淀剂和含有Mg Cl2,KCl,NaCl的盐水的混合物。从混合物中分离出氯化钠;获得莱昂石与氯化钾的沉淀混合物;过滤所说的Leonite,用水洗涤,得到Leonite与KCl的纯净混合物。用KCl将KCl加到Leonite中;并用KCl将Leonite分解为SOP。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号