首页> 外国专利> COMPOSITION AND SHAPING OF A CERAMIC MATERIAL WITH LOW THERMAL EXPANSION COEFFICIENT AND HIGH RESISTANCE TO THERMAL SHOCK

COMPOSITION AND SHAPING OF A CERAMIC MATERIAL WITH LOW THERMAL EXPANSION COEFFICIENT AND HIGH RESISTANCE TO THERMAL SHOCK

机译:低热膨胀系数和高抗热震性的陶瓷材料的组成和形状

摘要

The present invention is a composition and shaping of a ceramic material comprising at least one frit and at least one inorganic raw material. Some of the advantages are that said material requires a heat treatment no higher than 1180°C, that the duration of said heat treatment does not exceed 60 minutes, that the thermal expansion coefficient after the heat treatment is less than 25 x10-7 °C-1 in the temperature range 25 to 500°C and that the material exhibits a high resistance to thermal shock, withstanding at least 10 consecutive thermal shock cycles between 600 and 25°C without forming cracks or structural changes. The ceramic material composition is shaped by uniaxial pressing, band pressing, pour moulding, extrusion, injection moulding or lamination.
机译:本发明是一种陶瓷材料的组成和成形,该陶瓷材料包括至少一种玻璃料和至少一种无机原料。一些优点是,所述材料需要不高于1180℃的热处理,所述热处理的持续时间不超过60分钟,热处理之后的热膨胀系数小于25×10 -Sup-。在25至500°C的温度范围内为7 °C -1 ,并且该材料对热冲击具有很高的抵抗力,可以承受600至25°之间的至少10个连续的热冲击循环C不会形成裂纹或结构变化。陶瓷材料组合物通过单轴压制,带压,浇铸,挤出,注塑或层压而成形。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号