Prevents delayed cracking during drawing of high strength steel

机译:防止高强度钢拉伸过程中延迟开裂

摘要

The present invention relates to the prevention of delayed cracking of metal alloys during drawing, which can result from hydrogen attack. The alloy is applied to components or components used in vehicles such as white, a vehicle frame, a body in a chassis or a panel.
机译:本发明涉及防止在拉伸过程中金属合金的延迟开裂,该延迟开裂可以由氢侵蚀引起。将该合金应用于车辆中使用的一种或多种部件,例如白色,车架,底盘或面板中的车身。