The present invention relates to a high softening point reformed asphalt waterproofing compound and a waterproofing method using the same capable of forming a waterproofing sheet by inputting a softening point increasing additive to basic reformed asphalt with a softening point of 85°C or more; being constructed at 200°C or less; and having low-temperature bending properties for elongation at -30°C or more. The present invention comprises: 40-80 wt% of the basic reformed asphalt melted at 150-200°C; and the softening point increasing additive which is manufactured by mixing 10-50 wt% of waste tire powder, 5-20 wt% of blast furnace slag fine powder, 1-5 wt% of gilsonite powder, and 2-10 wt% of an adhesion improving agent. The basic reformed asphalt includes: 40-60 wt% of aspha 5-20 wt% of natural aspha 5-15 wt% of polymer plastic; 5-20 wt% of an SBS polymer; 2-10 wt% of a specific fiber filler; 0.1-0.5 wt% of an UV stabilizer; and 0.1-0.5 wt% of an antioxidant. The present invention impregnates or constructs the high softening point reformed asphalt waterproofing compound with a glass fiber mesh or a glass paper on a waterproofing surface; forms a waterproofing coating sheet by impregnating the high softening point reformed asphalt waterproofing compound with the glass fiber mesh or the glass paper and spraying silica; and then constructs a waterproofing layer by adhering to and compressing the waterproofing coating sheet on the waterproofing surface with the high softening point reformed asphalt waterproofing compound.
机译:高软化点改性沥青防水化合物及其使用方法,涉及一种通过向软化点为85℃以上的基础改性沥青输入软化点提高添加剂而形成防水片的防水方法。在200°C或更低的温度下施工;并且具有在-30℃以上的伸长率的低温弯曲特性。本发明包括:40-80重量%的在150-200℃熔化的碱性重整沥青;和以及通过混合10-50重量%的废轮胎粉末,5-20重量%的高炉矿渣细粉,1-5重量%的硅灰石粉和2-10重量%的硅酸盐粉末而制备的软化点增加添加剂。附着力改善剂。基本的重整沥青包括:40-60重量%的沥青; 5-20 wt%的天然沥青; 5-15 wt%的聚合物塑料; 5-20重量%的SBS聚合物; 2-10 wt%的特定纤维填料; 0.1-0.5 wt%的紫外线稳定剂;和0.1-0.5重量%的抗氧化剂。本发明通过在防水表面上用玻璃纤维网或玻璃纸浸渍或构造高软化点改性沥青防水化合物。通过在玻璃纤维网或玻璃纸中浸渍高软化点改性沥青防水化合物并喷涂二氧化硅来形成防水涂料片。然后通过将高软化点改性沥青防水复合材料粘附并压缩在防水表面上的防水涂层上而构建防水层。

著录项

  • 公开/公告号KR101845316B1

    专利类型

  • 公开/公告日2018-05-18

    原文格式PDF

  • 申请/专利权人 OATMNC CO. LTD.;

    申请/专利号KR20170082005

  • 发明设计人 KWON BONG JU;

    申请日2017-06-28

  • 分类号C04B26/26;C04B14/02;C04B16/02;C04B18/14;C04B18/22;C04B24/26;E04B1/64;C04B103/60;C04B111/27;

  • 国家 KR