Provided is a method for manufacturing a ceramic long fiber using fly ash. The method for manufacturing a ceramic long fiber using fly ash comprises: a step of firstly manufacturing first rock powder by dry-grinding first rock; a step of secondly manufacturing the first rock powder by wet-grinding the first rock powder; a step of firstly manufacturing second rock powder by dry-grinding second rock; a step of secondly manufacturing second rock powder by wet-grinding the second rock powder; a step of dry-mixing fly ash powder, the first rock powder, and the second rock powder and manufacturing an amorphous melting body by melting and quenching the same; and a step of manufacturing a ceramic fiber by melting and spinning the amorphous melting body. The first rock includes higher Al_2O_3 and CaO contents than the second rock. The second rock includes higher K_2O and Na_2O contents than the first rock. The amorphous melting body includes 10-30 wt% of the first rock, 10-20 wt% of the second rock, and 60-80 wt% of the fly ash powder. The ceramic long fiber is manufactured by continuously spinning the firstly manufactured amorphous melting body at 100-3,000 rpm of winding speed by secondly re-melting the firstly manufactured amorphous melting body at 1,400°C in bushing and cooling the same at 1,350-1,380°C. The present invention simplifies a manufacturing process.
机译:提供了一种使用粉煤灰制造陶瓷长纤维的方法。利用粉煤灰制造陶瓷长纤维的方法包括:首先通过干磨第一岩石来制造第一岩石粉末的步骤;第二步骤是通过湿磨第一岩粉来制造第一岩粉。首先通过干磨第二岩石来制造第二岩石粉末的步骤;第二步骤是通过湿磨第二岩粉来制造第二岩粉。将粉煤灰粉,第一岩粉和第二岩粉进行干混,并通过将其熔融和淬火来制造非晶态熔融体的步骤;通过熔融和纺丝所述非晶态熔融体来制造陶瓷纤维的步骤。第一岩石比第二岩石具有更高的Al_2O_3和CaO含量。第二岩石比第一岩石具有更高的K_2O和Na_2O含量。无定形熔化体包括10-30重量%的第一岩石,10-20重量%的第二岩石和60-80重量%的粉煤灰粉末。通过将第一制造的非晶态熔融体在套管中于1400℃下再熔融并在1350-1380℃下冷却,通过以100-3000rpm的卷绕速度连续纺制第一制造的非晶态熔融体来制造陶瓷长纤维。 。本发明简化了制造过程。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号