首页> 外国专利> METHOD AND CHARGE FOR PRODUCTION OF NITRATED SILICO-MANGANESE IN ARC ORE-THERMAL FURNACE

METHOD AND CHARGE FOR PRODUCTION OF NITRATED SILICO-MANGANESE IN ARC ORE-THERMAL FURNACE

机译:在电弧矿热炉中生产硝化硅锰的方法和费用

摘要

FIELD: metallurgy.;SUBSTANCE: method involves preparing and loading manganese ore and/or manganese concentrate and reducing mixture into the furnace, reducing melting and nitriding. Quartzite, dolomite, coke and/or coal and waste of carbide-silicon lining of aluminium electrolyzers containing silicon nitride are used as a reducing mixture. Reducing melting and nitriding are carried out simultaneously. Wastes of carbide-silicon lining of aluminium electrolyzers containing up to 70% of silicon carbide and up to 26% of silicon nitride are used. The charge contains, wt %: manganese ore and/or manganese concentrate 54.1-62.5; quartzite up to 9.9; coke and/or coal up to 6.8; dolomite 5.4-6.2; wastes of carbide-silicon lining 23.8-31.2.;EFFECT: invention makes it possible to increase the degree of manganese reduction in the alloy and reduce manganese content in the slag and simultaneously conduct nitriding of silico-manganese.;3 cl, 6 ex
机译:领域:冶金;物质:该方法涉及制备和装载锰矿石和/或锰精矿,并将混合物还原到炉中,以减少熔融和氮化。含有氮化硅的铝电解槽的石英石,白云石,焦炭和/或煤以及碳化硅衬里的废料被用作还原性混合物。还原熔融和氮化同时进行。使用了铝电解槽的碳化硅衬里的废料,其中含有多达70%的碳化硅和多达26%的氮化硅。装料包含以重量%计的锰矿石和/或锰精矿54.1-62.5;和石英岩可达9.9;焦炭和/或煤炭不超过6.8;白云石5.4-6.2;碳化硅衬里的废料23.8-31.2。效果:本发明可以提高合金中锰的还原度,降低炉渣中的锰含量,同时进行硅锰的氮化。3 cl,6 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号