FIELD: mining industry.;SUBSTANCE: invention relates to the processing of the mining industry solid low-level waste, namely, to the uranium extraction from a rock with the uranium content of 0.005–0.04 %. Method includes the uranium leaching using the thionic microorganisms association. At that, the leaching is carried out from the rock waste with a fraction of 1–40 mm with a ferric ions containing solution with a concentration of 10–25 g/l, divalent iron ions with a concentration of 0.5–5.0 g/l, a sulfuric acid solution with a concentration of 2–10 g/l, and the thionic microorganisms association microorganisms culture with the ferrooxidans predominant concentration. Leaching is carried out at pH value of 1.1–2.4 by percolation and bundle methods for 150–360 hours. At that, performing the trivalent iron solution regeneration with air oxygen, bubbled through the circulating solution, and the thionic bacteria association with the Acidithiobacillus ferrooxidans predominant content in a separate reactor.;EFFECT: technical result is an increase in the uranium leaching degree.;1 cl, 2 dwg, 1 ex, 2 tbl
机译:技术领域:本发明涉及采矿业固体低水平废物的处理,即涉及从铀含量为0.005-0.04%的岩石中提取铀。方法包括使用硫杂微生物协会进行铀浸出。那时,浸出是从含铁离子的溶液(浓度为10–25 g / l,含二价铁离子,浓度为0.5–5.0 g / l)中,在1–40 mm的碎石中进行的,浓度为2-10 g / l的硫酸溶液,硫离子微生物将微生物培养物与主要浓度的亚铁氧化物结合。通过渗滤和捆扎方法在pH值为1.1–2.4的条件下进行渗滤150–360小时。那时,用空气中的氧气进行三价铁溶液的再生,并在循环溶液中鼓泡,硫离子细菌与酸性铁氧体氧化亚铁的主要成分在一个单独的反应器中缔合。效果:技术成果是提高了铀的浸出度。 1厘升,2载重吨,1税前,2吨

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号