PROBLEM TO BE SOLVED: To restrain the occurrence of a spatter in pulse arc welding.;SOLUTION: In a pulse arc welding method using shield gas and a welding wire, a repeating welding period Tw includes a first period T1, a second period T2, and a third period T3. In the first period T1, a first peak current value Ip1 is supplied with a first pulse width of 10 msec or less as a welding current I. In the second period T2 following the first period T1, a second peak current value Ip2 having a larger current value than the first peak current value Ip1 is supplied with a second pulse width of 100 nsec or less as the welding current I. In the third period T3 following the second period T2, a base current value Ib having a smaller current value than the first peak current value Ip1 is supplied as the welding current I.;SELECTED DRAWING: Figure 4;COPYRIGHT: (C)2019,JPO&INPIT
机译:解决的问题:为了抑制脉冲电弧焊中飞溅的发生;解决方案:在使用保护气体和焊丝的脉冲电弧焊方法中,重复焊接周期T w 包括一个时间段T 1 ,第二时间段T 2 和第三时间段T 3 。在第一期间T 1 中,第一峰值电流值I p1 以10毫秒以下的第一脉冲宽度被提供作为焊接电流I。在第一周期T 1 之后的T 2 中,第二峰值电流值I p2 具有比第一峰值电流值I <为Sub> p1 提供100nsec或更小的第二脉冲宽度作为焊接电流I。在第二时段T 2 3 >,提供一个电流值小于第一峰值电流值I p1 的基本电流值I b 作为焊接电流I。版权:(C)2019,JPO&INPIT

著录项

  • 公开/公告号JP2019034333A

    专利类型

  • 公开/公告日2019-03-07

    原文格式PDF

  • 申请/专利权人 KOBE STEEL LTD;

    申请/专利号JP20170158981

  • 发明设计人 北村 佳昭;田尾 博昭;

    申请日2017-08-22

  • 分类号B23K9/09;

  • 国家 JP

  • 入库时间 2022-08-21 12:20:30

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号