PROBLEM TO BE SOLVED: To provide an aluminum fin material, a process of manufacture thereof, a heat exchanger, and an air conditioner capable of making harder to produce mold abrasion during press work while improving an antifouling property by making it difficult for both hydrophilic stain and hydrophobic stain to adhere.SOLUTION: An aluminum fin material of the invention includes an aqueous coating containing water soluble acryl resin containing alumina sol and sulfonic acid, and polyethylene glycol. A baked coating film of an aqueous coating material containing 5 to 45 mass% of alumina particles in 100 mass% of the coating solid content containing alumina particles in the alumina sol, the water soluble acryl resin, and the polyethylene glycol is formed on the surface of a plate composed of aluminum or an aluminum alloy; and the coating amount of the coating film is 0.3 to 0.8 g/m.SELECTED DRAWING: Figure 1
机译:解决的问题:提供一种铝翅片材料,其制造方法,热交换器和空调器,其能够通过使两种亲水性污渍都变得困难而在压制过程中更难以产生模具磨损,同时提高防污性。解决方案:本发明的铝翅片材料包括水性涂料,该水性涂料包含水溶性的丙烯酸树脂和聚乙二醇,该水溶性的丙烯酸树脂包含氧化铝溶胶和磺酸。在表面形成有水性涂料的烘焙涂膜,该水性涂料在氧化铝溶胶,水溶性丙烯酸树脂和聚乙二醇中的固形物含量为100质量%的情况下,包含5〜45质量%的氧化铝颗粒。由铝或铝合金组成的板;涂膜的涂布量为0.3至0.8 g / m。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号