摘要

The invention relates to a method for laminating a composite pane (100) without an autoclave, wherein: (a) a stack sequence (1) of a substrate pane (2), at least one intermediate layer (3), and a cover pane (4) is produced, (b1) a vacuum ring (5) or a vacuum bag is placed around the stack sequence (1), (b2) the stack sequence (1) is ventilated for a period of t ≥ 8 min and at a temperature T of 0 °C to 30 °C by applying a vacuum of p ≤ 0.3 bar to the vacuum ring (5) or the vacuum bag, (b3) the stack sequence (1) is heated to a temperature T of 70 °C to 115 °C , (b4) the stack sequence (1) is ventilated for a period t of t ≥ 8 min by applying a vacuum of p ≤ 0.3 bar to the vacuum ring (5) or the vacuum bag, (b5) the stack sequence (1) is cooled to a temperature T 70 °C, (b6) the vacuum ring (5) or the vacuum bag is supplied with air and removed, (c1) the stack sequence (1) is heated to a temperature T of 40 °C to 120 °C, and (c2) the stack sequence (1) is pressed together between at least two opposing calender rollers (6.1, 6.2) of a first calender unit (16) over the entire width b of the stack sequence (1).
机译:本发明涉及一种在没有高压釜的情况下层压复合板(100)的方法,其中:(a)基底板(2),至少一个中间层(3)和覆盖板的堆叠顺序(1)。产生(4),(b1)将真空环(5)或真空袋放在堆叠序列(1)周围,(b2)将堆叠序列(1)通风t≥8分钟,并在通过在真空环(5)或真空袋(b3)上施加p≤0.3 bar的真空,将温度T设置为0°C到30°C,将堆叠序列(1)加热到70°T C至115°C,(b4)通过在真空环(5)或真空袋(b5)上施加p≤0.3 bar的真空对t≥8分钟的时间t通风将堆叠序列(1)冷却至温度T <70°C,(b6)向真空环(5)或真空袋供气并取出,(c1)将堆叠序列(1)加热至温度T在40°C到120°C之间,并且(c2)堆叠顺序(1)在在堆叠序列(1)的整个宽度b上,第一压光单元(16)的两个相对的压光辊(6.1、6.2)向东。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号