PROBLEM TO BE SOLVED: To provide a photocurable resin molded body that features superior strength as well as reduced thickness and retardation, a polarizing plate using the same, and a transmissive liquid crystal display.SOLUTION: A photocurable resin molded body is obtained by photocuring a photocurable composition containing a photocurable resin and ultraviolet polymerization initiator, the photocurable resin comprising two types of acrylates A, B having two or three (meth)acryloyl groups. The acrylate A has a urethane skeleton and an aromatic ring or alicyclic structure, and exhibits a tensile strength of no less than 40 N/mmand tensile elongation of 3-10%, inclusive, when made into the resin molded body alone. The acrylate B exhibits a tensile strength of 5-35 N/mm, inclusive, and tensile elongation of no less than 30% when made into the resin molded body alone. A weight ratio of the acrylate A to acrylate B shall be in a range of 90:10 to 10:90. The photocurable resin molded body has a thickness of 15-50 μm, inclusive.SELECTED DRAWING: None
机译:要解决的问题:提供一种具有优异的强度并减小厚度和延迟的光固化树脂模制体,使用该光固化树脂模制体的偏振片和透射型液晶显示器。包含光固化性树脂和紫外线聚合引发剂的光固化性组合物,该光固化性树脂包含具有两个或三个(甲基)丙烯酰基的两种丙烯酸酯A,B。丙烯酸酯A具有氨基甲酸酯骨架和芳香环或脂环结构,当单独制成树脂成型体时,具有不小于40N / mm的拉伸强度和3-10%(含)的拉伸伸长率。当单独制成树脂成型体时,丙烯酸酯B表现出5-35N / mm(包括端值)的拉伸强度,并且拉伸伸长率不小于30%。丙烯酸酯A与丙烯酸酯B的重量比应在90:10至10:90的范围内。光固化树脂成型体的厚度为15-50μm(含)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号