首页> 外国专利> Cubic boron nitride particle-containing monocrystalline diamond particles and manufacturing method thereof

Cubic boron nitride particle-containing monocrystalline diamond particles and manufacturing method thereof

机译:含立方氮化硼颗粒的单晶金刚石颗粒及其制造方法

摘要

Thereby providing single crystal diamond particles excellent in thermal stability. The monocrystalline diamond particles contain cubic boron nitride particles. Preferably, the cubic boron nitride particles are present inside and / or on the surface of the cubic boron nitride particle-containing monocrystalline diamond particles, the average particle diameter of the monocrystalline diamond particles is 500 m or less, and the cubic boron nitride particles Has an average particle diameter of 0.05 to 100 m.
机译:从而提供热稳定性优异的单晶金刚石颗粒。单晶金刚石颗粒包含立方氮化硼颗粒。优选地,立方氮化硼颗粒存在于含立方氮化硼颗粒的单晶金刚石颗粒的内部和/或表面上,单晶金刚石颗粒的平均粒径为500m或更小,并且立方氮化硼颗粒具有平均粒径为0.05至100m。

著录项

  • 公开/公告号JPWO2018185909A1

    专利类型

  • 公开/公告日2019-04-18

    原文格式PDF

  • 申请/专利权人 大島 龍司;崔 祥仁;

    申请/专利号JP20170534859

  • 发明设计人 大島 龍司;崔 祥仁;

    申请日2017-04-06

  • 分类号C01B32/25;C30B29/04;B01J3/06;

  • 国家 JP

  • 入库时间 2022-08-21 12:18:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号