To improve cycling characteristics of a non-aqueous electrolyte secondary battery by obtaining a nickel-cobalt composite hydroxide having a sharp particle size distribution as a precursor, a slurry including a nickel-cobalt composite hydroxide obtained by continuously supplying an aqueous solution that includes at least nickel and cobalt, an ammonium ion donor aqueous solution and a caustic alkali aqueous solution to a reaction vessel and reacting, is continuously extracted and separated into a large particle size portion and s small particle size portion by classification, and the small particle size portion is continuously returned to the reaction vessel. As a result, a nickel-cobalt composite hydroxide is obtained that is expressed by the general formula: Ni1-x-yCoxMy(OH)2 (where, 0.05≤x≤0.50, 0≤y≤0.10, 0.05≤x+y≤0.50, and M is at least one kind of metal element selected from among Al, Mg, Mn, Ti, Fe, Cu, Zn and Ga, and that satisfies the relationships (D50−D10)/D50≤0.30, and (D90−D50)/D50≤0.30 among D10, D50 and D90 of this composite hydroxide.
机译:为了通过获得具有尖锐的粒度分布的镍-钴复合氢氧化物作为前体来改善非水电解质二次电池的循环特性,包含通过连续供应至少包含至少10%的水溶液而获得的包含镍-钴复合氢氧化物的浆料。通过分级将镍和钴,铵离子供体水溶液和苛性碱水溶液进行反应并连续萃取,并通过分级将其分离成大粒径部分和小粒径部分。连续返回到反应容器中。结果,获得了镍-钴复合氢氧化物,其由以下通式表示:Ni 1-xy Co x M y ( OH) 2 (其中0.05≤x≤0.50、0≤y≤0.10、0.05≤x +y≤0.50,并且M是选自Al,Mg, Mn,Ti,Fe,Cu,Zn和Ga满足该复合氢氧化物的D10,D50和D90之间的(D50-D10)/D50≤0.30和(D90-D50)/D50≤0.30的关系。

著录项

  • 公开/公告号US10141571B2

    专利类型

  • 公开/公告日2018-11-27

    原文格式PDF

  • 申请/专利权人 SUMITOMO METAL MINING CO. LTD.;

    申请/专利号US201314431995

  • 申请日2013-09-27

  • 分类号H01M4/525;C01G53;B01J19/24;H01M4/04;H01M10/0525;H01M4/02;

  • 国家 US

  • 入库时间 2022-08-21 12:08:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号