Provided is a method for manufacturing a round billet of Ni-containing high alloy including steps of continuously casting a molten steel by using a casting mold, thereby obtaining a rectangular billet, and shaping the rectangular billet into round billet by forging/rolling, wherein the casting mold has a shape such that a w/h ratio between long side length (w) and short side length (h) of a cross section of the rectangular billet perpendicular to the casting direction of rectangular billet is 1.0 to 2.0, the chemical composition of molten steel is, by mass %: C: 0.005 to 0.250%, Si: 0.05 to 2.00%, Mn: 0.05 to 3.00%, P: 0.04% or less, S: 0.004% or less, Cu: 0.01 to 3.00%, Cr: 10 to 35%, Ni: 10 to 80%, Mo: 1.5 to 10.0%, Al: 0.001 to 0.300%, N: 0.001 to 0.300%, W: 0.00 to 6.00%, Ti: 0.00 to 2.00%, and the balance: Fe and impurities.
机译:提供一种制造含Ni高合金圆坯的方法,该方法包括以下步骤:通过使用铸模连续浇铸钢水,从而获得矩形坯,并且通过锻造/轧制将矩形坯成形为圆形坯。铸模具有这样的形状,使得与矩形坯料的浇铸方向垂直的矩形坯料的横截面的长边长度(w)与短边长度(h)之间的w / h比为1.0至2.0,以质量%计:C:0.005〜0.250%,Si:0.05〜2.00%,Mn:0.05〜3.00%,P:0.04%以下,S:0.004%以下,Cu:0.01〜3.00%, Cr:10至35%,Ni:10至80%,Mo:1.5至10.0%,Al:0.001至0.300%,N:0.001至0.300%,W:0.00至6.00%,Ti:0.00至2.00%,和余量:铁和杂质。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号