Process for the manufacture of a body and low energy reference proof for the Charpy impact test and reference body thus obtained. This invention refers to a process for the manufacture of a low -energy test body for a Charpy impact test comprising a heat treatment step (300) with simple and low -complexity sub -steps (310 to 360),And provides a low -energy reference body that can be tested at room temperature. The heat treatment step (300) proposed by this invention comprises the heating of a steel bar at approximately 900 0C temperature for approximately 60 mm. (310);The air bar cooler (320);A new heat step of the bar at a temperature of approximately 870 0C by about 60 mm. (330);The temperature of the oil bar (340);The revenged at a temperature about 300 0C by about 120 mm. (350) and new oil rod tempering (360).
机译:由此获得用于夏比冲击试验的物体和低能量参考证明的制造方法以及参考物体。本发明涉及一种用于夏比冲击试验的低能量试验体的制造方法,其包括具有简单和低复杂度子步骤(310至360)的热处理步骤(300),并且提供了一种低能量可以在室温下测试的参考体。本发明提出的热处理步骤(300)包括在大约900 0℃的温度下将钢筋加热大约60mm。 (310);空气棒冷却器(320);在大约870 0C的温度下,将棒进行新的加热约60毫米。 (330);油条的温度(340);在大约300 0C的温度下改变了大约120毫米。 (350)和新的油杆回火(360)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号