The invention relates to a method of heat treatment of sulfur-containing ore, in which the ore is calcined at temperatures from 600 to 1200 ° C in the presence of oxygen in the reactor so that from 1 to 90 wt.% Sulfur contained in the ore is burned to sulfur dioxide, and the impurities contained removed in gaseous form. The resulting waste gas containing sulfur dioxide is fed to a gas purification system comprising at least one component, and / or the burnt ore is fed to at least one additional process stage. The exhaust gas from the gas cleaning and / or the specified process stage and / or the gas used for cooling during gas cleaning or for cooling in an additional process stage is at least partially returned back to the reactor as recycle gas having a temperature of 100 ° C.
机译:本发明涉及一种热处理含硫矿石的方法,其中在反应器中存在氧气的情况下在600至1200℃的温度下煅烧矿石,以使含硫矿石中所含的硫为1至90重量%。矿石燃烧成二氧化硫,并以气态形式除去杂质。将所得的包含二氧化硫的废气进料至包含至少一种组分的气体净化系统,和/或将燃烧的矿石进料至至少一个另外的工艺阶段。来自气体清洁和/或指定的处理阶段的废气和/或用于气体清洁过程中冷却或用于其他过程阶段的冷却的气体至少部分返回到反应器,温度为> 100℃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号