The purpose of the notification is the production of a spray paint for coatings with a high resistance to the action of essential oils containing as a base,aqueous polyurethane dispersion,consisting of doses of 59% to 60%m /m /polyurethane dispersion of the active substance from 30 to 35%m /m, in which the urethane polymer is silicone -modified, to the water -coated mixer and the quick -boiler the temperature from 30oC to 35oC and the whole is mixed and, during continuous mixing, added as follows: from 0,1% to 1,0%m /m emulsion of the polyetheroxyloxane copolymer in water with dry mass content from 20% to 25%m, from 0,05% to 0,3%m /m of a potent air pressure reducing agent polyether -modified polydimethylsiloxane, 0,04% to 0,15% m /m,favourable 0,1%m /m biocidal product in the form of a dispersion containing the active substances: methylisothiazolinone and iodopropynylobutyl carbamate (3 -iodo -2 -propynyl butyl carbamate) mixed in relation to 3:1, increasing the turnover of the mixture and homogenising the mixture and then adding water which is de -mineralised in the quantity resulting from the additives and then dosed with 0,01% to 0,5%m /m of silicon which has been tempered, the pre -homogenised mixture is subjected to a cavitation process and is dynamically cooled to a temperature after switching to a cavity mixture hours from 10oC to 15oC.
机译:通报的目的是生产一种涂料,该涂料具有很高的抗香精油作用的涂料的性能,该涂料含有59%至60%m / m /聚氨酯分散体的聚氨酯水分散体作为基础。将30%至35%m / m的活性物质(其中氨基甲酸酯聚合物进行了有机硅改性)在30°C至35oC的温度下向水涂布混合器和速沸器中进行混合,并在连续混合过程中添加如下:聚醚氧基氧烷共聚物在水中的0.1%至1,0%m / m的乳液,干质量含量为20%至25%m,0.05%至0.3%m / m强力的减压剂聚醚改性的聚二甲基硅氧烷,0.04%至0.15%m / m,有利的0.1%m / m杀生物产品,其分散液形式含有以下活性物质:甲基异噻唑啉酮和碘代丙炔基丁基氨基甲酸酯(3 -碘-2-氨基甲酸丙炔基丁酯)相对于3:1混合,增加了混合物的周转率e,均化混合物,然后加入水,该水以添加剂产生的量进行软化处理,然后加入0.01%至0.5%m / m的硅,并进行回火,预均质的混合物为进行空化过程,并在从10oC到15oC切换到型腔混合物后动态冷却到一定温度。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号