The invention relates to an oxygen carrier solid, its preparation and its use in a method of combustion of a hydrocarbon feedstock by active mass chemical-looping oxidation-reduction, i.e. chemical-looping combustion (CLC). The solid, which is in the form of particles, comprises an oxidation-reduction active mass composed of metal oxide(s) dispersed in a ceramic matrix comprising at least at least one feldspar or feldspathoid with a melting point higher than 1500°C, such as celsian, and has, initially, a specific macroporous texture. The oxygen carrier solid is prepared from a precursor of the ceramic matrix, obtained from a macroporous zeolitic material with zeolite crystals of a specific size, and a precursor of the oxidation-reduction active mass.
机译:氧载体固体,其制备及其在通过活性物质化学环氧化还原即化学环燃烧(CLC)燃烧烃原料的方法中的用途。呈颗粒形式的固体包含由金属氧化物组成的氧化还原活性物质,所述金属氧化物分散在陶瓷基质中,所述陶瓷基质包含至少一种熔点高于1500℃的长石或长石类,像celsian,最初具有特定的大孔纹理。氧载体固体由陶瓷基质的前体和氧化还原活性物质的前体制备,所述前体是从具有特定尺寸的沸石晶体的大孔沸石材料中获得的。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号