Provided is a preparation method of a 1Cr17 ferritic stainless steel pipe. The method comprises the following steps: preheating a 1Cr17 ferritic stainless steel pipe billet and keeping at the temperature; perforation to obtain a hot-rolled perforated tube, wherein the chemical element and mass % ratio of the steel pipe is as follows: 0.08-0.12% of carbon, ≤0.04% of silicon, ≤0.70% of manganese, 16.40-17.00% of chrome, ≤0.035% of phosphorus, ≤0.010% of sulfur and the balance iron; performing thermal refining on the obtained hot-rolled perforated pipe to obtain a perforated pipe; performing normal-temperature cold rolling on the obtained perforated pipe to obtain a cold rolled pipe; and performing thermal treatment on the cold rolled pipe, cooling the same to normal temperature after thermal treatment is finished, and a finished product is obtained.
机译:提供一种1Cr17铁素体不锈钢管的制备方法。该方法包括以下步骤:预热1Cr17铁素体不锈钢管坯并保持该温度;穿孔以获得热轧穿孔管,其中钢管的化学元素和质量百分比如下:碳0.08-0.12%,硅≤0.04%,锰≤0.70%,锰16.40-17.00%铬,磷≤0.035%,硫≤0.010%,余量铁;对得到的热轧多孔管进行热精炼,得到多孔管。对得到的多孔管进行常温冷轧,从而得到冷轧管。对冷轧管进行热处理,热处理结束后,冷却至常温,得到成品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号