SEMI-AROMATIC POLYAMIDE, PREPARATION METHOD THEREOF, AND POLYAMIDE MOLDING COMPOSITION CONTAINING SAID SEMI-AROMATIC POLYAMIDE

机译:半芳族聚酰胺,其制备方法以及包含所述半芳族聚酰胺的聚酰胺模塑组合物

摘要

The present invention relates to a semi-aromatic polyamide resin, a preparation method thereof, and a polyamide molding composition containing said semi-aromatic polyamide resin. The content of isolated terephthalic acid in the semi-aromatic polyamide resin is less than 500 ppm. Said semi-aromatic polyamide resin consists of the following repeating units: (a) a terephthalic acid or a derivative thereof, and optionally one or more additional aromatic or aliphatic diacids; (b) one or more aliphatic diamines having 10-20 carbon atoms, and optionally one or more additional diamines; (c) optionally one or more amino carboxylic acids and/or lactam, wherein the terephthalic acid accounts for 50-100 mol % of (a), and one or more aliphatic diamines have 10-20 carbon atoms accounting for 50-100 mol % in the aliphatic diamines (b), and the one or more amino carboxylic acids and/or lactam account for 0-25 mol % of the total amount of (a) + (b) + (c). The disclosed semi-aromatic polyamide resin may improve the melting process by solving problems related to, for example but not limited to, gas and products pollution.
机译:半芳族聚酰胺树脂,其制备方法以及包含该半芳族聚酰胺树脂的聚酰胺成型用组合物技术领域半芳族聚酰胺树脂中的分离对苯二甲酸的含量小于500ppm。所述半芳族聚酰胺树脂由以下重复单元组成:(a)对苯二甲酸或其衍生物,以及任选地一种或多种另外的芳族或脂族二酸; (b)一种或多种具有10-20个碳原子的脂族二胺,和任选地一种或多种另外的二胺; (c)任选地一种或多种氨基羧酸和/或内酰胺,其中对苯二甲酸占(a)的50-100mol%,并且一种或多种脂族二胺具有10-20个碳原子,占50-100mol%在脂肪族二胺(b)中,一种或多种氨基羧酸和/或内酰胺占(a)+(b)+(c)总量的0-25mol%。所公开的半芳族聚酰胺树脂可以通过解决与例如但不限于气体和产品污染有关的问题来改善熔融过程。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号