A supercritical carbon dioxide-assisted solid-phase grafting modification method for polypropylene, comprises swelling polypropylene for 0.5 to 10 hours in supercritical carbon dioxide having dissolved vinyl monomer and an initiator, then slowly relieving the pressure; moving the polypropylene that has undergone the swelling process into a reaction kettle, and adding xylene as an interface agent, the mass of xylene being 1% of the polypropylene; increasing the temperature to between 65°C and 165°C under normal pressure, and reacting 1 to 10 hours to obtain modified polypropylene; the swelling permeation temperature during the swelling process is from 31°C to 60°C, the swelling pressure is from 7.5 to 12 MPa; the initiator is an azo compound or a peroxide. In the present method, the grafting rate reaches 5.4%, the thermal property, polarity, and mechanical property all improve substantially, and hydrophilic property is substantially enhanced.
机译:一种用于聚丙烯的超临界二氧化碳辅助固相接枝改性方法,包括在具有溶解的乙烯基单体和引发剂的超临界二氧化碳中将聚丙烯溶胀0.5至10小时,然后缓慢释放压力。将经过溶胀处理的聚丙烯移至反应釜中,并加入二甲苯作为界面剂,二甲苯的质量为聚丙烯的1%。在常压下将温度升至65℃至165℃,反应1至10小时,得到改性聚丙烯。溶胀过程中的溶胀渗透温度为31℃至60℃,溶胀压力为7.5至12MPa。引发剂是偶氮化合物或过氧化物。在本方法中,接枝率达到5.4%,热性能,极性和机械性能均显着改善,并且亲水性显着提高。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号