The purpose of/problem addressed by the present invention is to provide: an Fe(II)-substituted MEL-type zeolite useful for the catalytic removal of a variety of gases; and a production method therefor. The SiO 2 /Al 2 O 3 ratio in this Fe(II)-substituted MEL-type zeolite is in the range of 10-30 inclusive. This Fe(II)-substituted MEL-type zeolite is obtained by being subjected to ionic exchange with Fe(II) ions. It is preferable that the Fe(II) loading amount be in the range of 0.001-0.4mmol/g of the Fe(II)-substituted MEL-type zeolite. It is preferable that the Fe(II)-substituted MEL-type zeolite be produced using a method in which an MEL-type zeolite having an SiO 2 /Al 2 O 3 ratio in the range of 10-30 inclusive is dispersed in an Fe(II) water-soluble-compound aqueous solution, and then mixed and agitated to cause the MEL-type zeolite to carry Fe(II) ions.
机译:本发明解决的目的/问题是提供:用于催化除去各种气体的Fe(II)取代的MEL型沸石;和及其制造方法。该Fe(II)取代的MEL型沸石中的SiO 2 / Al 2 O 3的比例为10以上且30以下。该Fe(II)取代的MEL型沸石是通过与Fe(II)离子进行离子交换而获得的。 Fe(II)的负载量优选为0.001-0.4mmol / g的Fe(II)-取代的MEL-型沸石。 Fe(II)取代的MEL型沸石优选使用将SiO 2 / Al 2 O 3比为10〜30的范围的MEL型沸石分散在Fe中的方法来制造。 (II)水溶性化合物水溶液,然后混合并搅拌以使MEL型沸石携带Fe(II)离子。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号