A low-reflection coated glass sheet of the present invention includes a glass sheet and a low-reflection coating. The low-reflection coating is formed on at least a portion of one principal surface of the glass sheet and contains a binder containing silica as a main component, fine silica particles bound by the binder, and fine titania particles bound by the binder. The low-reflection coating satisfies the following relationships: 30 mass% C 68 mass%; 12 mass% ≤ C 50 mass%; 20 mass% C≤ 43.75 mass%; C/C≥ 0.6; C 25 mass% in the case of Csp ≥ 55 mass%; and C 20 mass% in the case of C 55 mass%The low-reflection coated glass sheet has a transmittance gain of 2.0% or more.
机译:本发明的低反射涂层玻璃板包括玻璃板和低反射涂层。低反射涂层形成在玻璃板的一个主表面的至少一部分上,并且包含以二氧化硅为主要成分的粘合剂,通过粘合剂结合的二氧化硅细颗粒和通过粘合剂结合的二氧化钛细颗粒。低反射涂层满足以下关系:30质量%<C <68质量%; 12质量%≤C<50质量%; 20质量%<C≤43.75质量%; C /C≥0.6; Csp≥55质量%时,C <25质量%。 C <55质量%的情况下,C> 20质量%的低反射镀膜玻璃板的透射率增加为2.0%以上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号