首页> 外国专利> FE-NI-CR ALLOY, FE-NI-CR ALLOY STRIP, SHEATH HEATER, METHOD FOR PRODUCING FE-NI-CR ALLOY, AND METHOD FOR PRODUCING SHEATH HEATER

FE-NI-CR ALLOY, FE-NI-CR ALLOY STRIP, SHEATH HEATER, METHOD FOR PRODUCING FE-NI-CR ALLOY, AND METHOD FOR PRODUCING SHEATH HEATER

机译:FE-NI-CR合金,FE-NI-CR合金钢带,护套加热器,制造FE-NI-CR合金的方法以及护套加热器的方法

摘要

Provided is an Fe-Ni-Cr alloy that has excellent surface characteristics and enables formation of a blackened coating having excellent blackening characteristics and peeling resistance. The Fe-Ni-Cr alloy has a chemical composition containing, by mass%, C, Si, Mn, P, S, Cr, Ni, Mo, Co, Cu, N, Ti, Al, O, and H, the balance being Fe and inevitable impurities, and satisfying formulae (1) to (4): (1) T1 = 11 × [%N] + 0.1; (2) T2 = -39 × [%N] + 1.0; (3) A1 = 7.5 × [%N] + 0.1; (4) A2 = -42.5 × [%N] + 1.0, where [%M] represents content (mass%) of element M in the alloy, and T1, T2, A1, and A2 satisfy relationships T1 [%Ti] T2 and A1 [%Al] A2.
机译:提供了一种Fe-Ni-Cr合金,其具有优异的表面特性并且能够形成具有优异的发黑特性和耐剥离性的发黑涂层。 Fe-Ni-Cr合金具有以质量%计包含C,Si,Mn,P,S,Cr,Ni,Mo,Co,Cu,N,Ti,Al,O和H的化学组成。为Fe且不可避免的杂质,满足式(1)〜(4):(1)T1 = 11×[%N] +0.1。 (2)T2 = -39×[%N] + 1.0; (3)A1 = 7.5×[%N] + 0.1; (4)A2 = -42.5×[%N] + 1.0,其中[%M]表示合金中元素M的含量(质量%),且T1,T2,A1和A2满足关系T1 <[%Ti]

著录项

  • 公开/公告号EP3467137A4

    专利类型

  • 公开/公告日2019-11-20

    原文格式PDF

  • 申请/专利权人 NIPPON YAKIN KOGYO CO. LTD.;

    申请/专利号EP20170806125

  • 申请日2017-03-14

  • 分类号C22C38/58;C21D1/76;C21C7/04;C21C7/072;C21C7/076;H05B3/48;C21C7/064;C21D9/46;C22C38;C22C38/02;C22C38/04;C22C38/42;C22C38/44;C22C38/50;C22C38/52;

  • 国家 EP

  • 入库时间 2022-08-21 11:39:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号