VINYLPYRIDINE RESIN FOR CATALYST SUPPORTS, PRODUCTION METHOD THEREFOR, AND CATALYST FOR METHANOL CARBONYLATION REACTION

机译:用于催化剂支持的维尼丁树脂,其制备方法和用于甲醇羰基化反应的催化剂

摘要

A vinylpyridine resin for a catalyst support; a method for producing thereof; and a catalyst for carbonylation of methanol are disclosed. The vinylpyridine resin has: content of nitrogen derived from a pyridine group of 3.00% by mass or more and 8.00% by mass or less; degree of crosslinking of 35% by mole or more and 70% by mole or less; molar ratio C/N of carbon atoms to nitrogen atoms of 12.00 or more and 36.00 or less; total pore volume of 0.20 cc/g or more and 0.45 cc/g or less; specific surface area of 70.0 m2/g or more and 280 m2/g or less; average pore diameter of 5.0 nm or more and 25.0 nm or less; and proportion of a volume of pores having a pore diameter of 10 nm or more to a volume of the whole pores of 4.0% or more and 90.0% or less.
机译:用于催化剂载体的乙烯基吡啶树脂;其生产方法;公开了一种用于甲醇羰基化的催化剂。乙烯基吡啶树脂具有:3.00质量%以上且8.00质量%以下的来自吡啶基的氮的含量;交联度为35摩尔%以上且70摩尔%以下。碳原子与氮原子的摩尔比C / N为12.00以上且36.00以下。总孔体积为0.20cc / g以上且0.45cc / g以下;比表面积为70.0m 2 / g以上且280m 2 / g以下;平均孔径为5.0nm以上且25.0nm以下;孔径为10nm以上的细孔的体积相对于全部细孔的体积为4.0%以上90.0%以下的比例。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号