An object of the present invention is to provide nickel cobalt manganese composite hydroxide particles having a small particle diameter and a uniform particle size distribution, and a method for producing the same. A method for producing a nickel cobalt manganese composite hydroxide by a crystallization reaction is provided. The method includes: a nucleation step of performing nucleation by controlling a pH of an aqueous solution for nucleation including metal compounds containing nickel, cobalt and manganese, and an ammonium ion donor to 12.0 to 14.0 in teams of the pH as measured at a liquid temperature of 25° C. as a standard; and a particle growth step of growing nuclei by controlling a pH of an aqueous solution for particle growth containing nuclei formed in the nucleation step to 10.5 to 12.0 in terms of the pH as measured at a liquid temperature of 25° C. as a standard.
机译:本发明的目的是提供粒径小且粒径分布均匀的镍钴锰复合氢氧化物粒子及其制造方法。提供了一种通过结晶反应生产镍钴锰复合氢氧化物的方法。该方法包括:成核步骤,该成核步骤通过控制用于成核的水溶液的pH来进行成核,该水溶液包括在液体温度下测量的pH值,该成核水溶液包含pH值的团队,该金属化合物包含镍,钴和锰以及铵离子供体,pH值为12.0至14.0。以25℃为标准;通过将含有在成核步骤中形成的核的,以在25℃的液体温度下测量的pH为基准的粒子生长用水溶液的pH控制为10.5至12.0,来生长核的粒子生长步骤。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号