A cold-rolled steel sheet containing: in mass%, C: 0.0005 to 0.0045%; Mn: 0.80 to 2.50%; Ti: 0.002 to 0.150%; B: 0.0005 to 0.01%, in which (1) Expression is satisfied, and a balance being composed of iron and impurities, in which at the position of 1/4 thickness of a sheet thickness, a random intensity ratio (A) of the {332}110 orientation is 3 or less, a random intensity ratio (B) of the {557}9 16 5 orientation and a random intensity ratio (C) of the {111}112 orientation are both 7 or more, and {(B)/(A) ‰§ 5} and {(B) (C)} are satisfied.
机译:一种冷轧钢板,其中,以质量%计,C:0.0005〜0.0045%; C:0.0005〜0.0045%。 Mn:0.80〜2.50%。 Ti:0.002〜0.150%。 B:0.0005〜0.01%,其中,(1)满足表达式,并且由铁和杂质构成的平衡,其中,在片材厚度的1/4厚度的位置处,B的随机强度比(A)为B。 {332} <110>方向为3或更小,{557} <9 16 5>方向的随机强度比(B)和{111} <112>方向的随机强度比(C)均为7大于或等于{(B)/(A)≥5}和{(B)>(C)}。

著录项

  • 公开/公告号PL2881483T3

    专利类型

  • 公开/公告日2020-02-28

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORPORATION;

    申请/专利号PL20130826234T

  • 申请日2013-07-31

  • 分类号C22C38/38;B32B15/01;C21D8/02;C21D8/04;C21D9/46;C22C38/02;C22C38/06;C22C38/08;C22C38/12;C22C38/18;C22C38/22;C23C2/28;C23C2/40;C25D5/36;C25D7/06;

  • 国家 PL

  • 入库时间 2022-08-21 11:16:42

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号