首页> 外国专利> Amorphous or semi-morph stainless steel or Ti-Al-C ceramic or Zr-Al-C ceramic kinetically applied with nuclear quality zirconium alloy metal structure

Amorphous or semi-morph stainless steel or Ti-Al-C ceramic or Zr-Al-C ceramic kinetically applied with nuclear quality zirconium alloy metal structure

机译:动态或具有核品质的锆合金金属结构的非晶态或半晶态不锈钢或Ti-Al-C陶瓷或Zr-Al-C陶瓷

摘要

A composition and method of kinetically depositing the composition to form a coating onto an exterior surface of a zirconium alloy cladding of a light water nuclear reactor which at least partially adheres to the exterior surface. The coating composition includes a first component and a second component. The first component is selected from the group consisting of zirconium, zirconium oxide and mixtures thereof. The second component is selected from the group consisting of Zr2AlC ceramic, Ti2AlC ceramic, Ti3AlC2 ceramic, Al2O3, aluminum, zirconium silicide, amorphous and semi-amorphous alloyed stainless steel, and mixtures of Zr2AlC ceramic, Ti2AlC ceramic and Ti3AlC2 ceramic. The coating has a gradient emanating from the exterior surface of the cladding toward an exposed outer surface of the coating such that percent by weight of the first component decreases and the second component increases from the exterior surface of the cladding toward the exposed outer surface of the coating.
机译:一种组合物和将组合物动力学沉积以在轻水核反应堆的锆合金覆层的外表面上形成涂层的方法,该涂层至少部分粘附于该外表面。该涂料组合物包含第一组分和第二组分。第一组分选自锆,氧化锆及其混合物。第二组分选自Zr2AlC陶瓷,Ti2AlC陶瓷,Ti3AlC2陶瓷,Al2O3,铝,硅化锆,非晶和半非晶合金不锈钢,以及Zr2AlC陶瓷,Ti2AlC陶瓷和Ti3AlC2陶瓷的混合物。涂层具有从包层的外表面朝向涂层的暴露的外表面发出的梯度,使得第一组分的重量百分比降低,第二组分从包层的外表面朝向涂层的暴露的外表面增加。涂层。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号