BINDER COMPOSITION FOR ALL-SOLID-STATE SECONDARY BATTERY, SLURRY COMPOSITION FOR ALL-SOLID-STATE SECONDARY BATTERY ELECTRODE MIXTURE LAYER, SLURRY COMPOSITION FOR ALL-SOLID-STATE SECONDARY BATTERY SOLID ELECTROLYTE LAYER, AND ALL-SOLID-STATE SECONDARY BATTERY

机译:全固态二次电池的粘合剂组合物,全固态二次电池电极混合物层的淤浆组成,全固态二次电池固体混合物的淤浆组成和全固态二次电池

摘要

The purpose of the present invention is to provide an all-solid-state secondary battery binder composition which can form a solid electrolyte-containing layer which, in an all-solid-state secondary battery, can exhibit excellent output characteristics and high-temperature cycle characteristics. This binder composition contains a polymer A; the polymer A contains nitrile group-containing monomer units and aliphatic conjugated diene monomer units; the content ratio of the nitrile group-containing monomer units in the polymer A is 5-30 mass%, the content ratio of the aliphatic conjugated diene monomer units is 40-95%, and the Mooney viscosity (ML1+4, 100°C) of the polymer A is greater than or equal to 65.
机译:本发明的目的是提供一种可以形成固体含电解质层的全固态二次电池粘合剂组合物,所述固体含电解质层在全固态二次电池中可以表现出优异的输出特性和高温循环。特征。该粘合剂组合物包含聚合物A。聚合物A含有含腈基的单体单元和脂肪族共轭二烯单体单元。聚合物A中的含腈基单体单元的含量比例为5〜30质量%,脂肪族共轭二烯单体单元的含量比例为40〜95%,门尼粘度(ML 1 + 4 ,则聚合物A的100°C大于或等于65。

著录项

  • 公开/公告号WO2020045226A1

    专利类型

  • 公开/公告日2020-03-05

    原文格式PDF

  • 申请/专利权人 ZEON CORPORATION;

    申请/专利号WO2019JP32834

  • 发明设计人 MATSUO YUSAKU;SONOBE KENYA;

    申请日2019-08-22

  • 分类号H01M10/0562;H01M4/139;H01M4/62;H01M10/052;H01M10/058;

  • 国家 WO

  • 入库时间 2022-08-21 11:13:08

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号