首页> 外国专利> METHOD FOR ESTIMATING COKE STRENGTH AFTER REACTION

METHOD FOR ESTIMATING COKE STRENGTH AFTER REACTION

机译:反应后焦炭强度的估算方法

摘要

A method of estimating the hot strength of coke with improved accuracy using factors related to the amount of coal components and hot properties of coal is provided. As a method for estimating the hot strength of coke used for manufacturing molten iron, the hot strength (CSR) of coke satisfies the following equation.CSR = -4.2O - 88.2Rm 2 + 185Rm + 1.85Ash 2 - 31Ash + 109.7 Here, O is the amount of oxygen contained in the coal used as coke (vol%), Rm is the reflectance of coal, and Ash is the amount of ash contained in the coal (wt%).
机译:提供了一种使用与煤成分的量和煤的热性质有关的因素以提高的精度估计焦炭的热强度的方法。作为估算用于生产铁水的焦炭热强度的一种方法,焦炭的热强度(CSR)满足以下公式: CSR = -4.2O-88.2Rm 2 + 185Rm + 1.85Ash 2-31Ash + 109.7在此,O是用作焦炭的煤中的氧气含量(体积%),Rm是煤的反射率,Ash是煤中的煤灰含量(wt%)。

著录项

  • 公开/公告号KR20200119077A

    专利类型

  • 公开/公告日2020-10-19

    原文格式PDF

  • 申请/专利权人 포항공과대학교 산학협력단;

    申请/专利号KR1020190041453

  • 发明设计人 김성만;김장규;

    申请日2019-04-09

  • 分类号G01N33/22;C10B45;

  • 国家 KR

  • 入库时间 2022-08-21 11:05:49

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号