首页> 外国专利> ANNEALING SEPARATING AGENT COMPOSITION FOR GRAIN ORIENTED ELECTRICAL STEEL SHEET METHOD FOR MANUFACTURING MAGNESIUM OXIDE FOR ANNEALING SEPARATING AGENT AND METHOD FOR MANUFACTURING GRAIN ORIENTED ELECTRICAL STEEL SHEET

ANNEALING SEPARATING AGENT COMPOSITION FOR GRAIN ORIENTED ELECTRICAL STEEL SHEET METHOD FOR MANUFACTURING MAGNESIUM OXIDE FOR ANNEALING SEPARATING AGENT AND METHOD FOR MANUFACTURING GRAIN ORIENTED ELECTRICAL STEEL SHEET

机译:晶粒取向电工钢板的退火分离剂成分的制造氧化镁的退火分离剂的制备方法

摘要

The annealing separator composition for a grain-oriented electrical steel sheet according to an embodiment of the present invention includes magnesium oxide, and the hydration water slope of magnesium oxide represented by the following Formula 1 is 0.28 to 0.50. [Equation 1] [Hydration Moisture Gradient] = ([Ig.loss2]-[Ig.loss1]) / ([T2]-[T1]) (In Formula 1, [Ig.loss1] and [Ig.loss2] are the weight loss rate (% by weight) of magnesium oxide when the hydrated magnesium oxide is raised to the temperature of [T1] and [T2], respectively, [T1] and [T2] is the temperature (° C.) selected at 550 to 1000 ° C. respectively. [T1] and [T2] are different from each other.)
机译:根据本发明的实施方式的用于方向性电磁钢板的退火隔离剂组合物包含氧化镁,并且由下式1表示的氧化镁的水合水斜率是0.28至0.50。 [等式1] [水合水分梯度] =([Ig.loss2]-[Ig.loss1])/([T2]-[T1])(在公式1中,[Ig.loss1]和[Ig.loss2]为将水合氧化镁分别升高到[T1]和[T2]的温度时的氧化镁的失重率(重量%),[T1]和[T2]是在以下条件下选择的温度(℃)分别为550至1000°C。[T1]和[T2]互不相同。)

著录项

  • 公开/公告号KR102080168B1

    专利类型

  • 公开/公告日2020-02-21

    原文格式PDF

  • 申请/专利权人 주식회사 포스코;

    申请/专利号KR20170179233

  • 发明设计人 한민수;박창빈;김윤수;박종태;

    申请日2017-12-26

  • 分类号C21D8/12;C01F5/08;C21D1/68;

  • 国家 KR

  • 入库时间 2022-08-21 11:05:14

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号