The present invention relates to a catalytic cracking catalyst and a method for preparing the same, wherein the catalytic cracking catalyst comprises a catalytic cracking active ingredient, an optional mesoporous aluminosilicate material, a clay and a binder, wherein the catalytic cracking active ingredient is a rare earth-containing Y type The rare earth-containing Y-type zeolite comprising, consisting of, or consisting essentially of zeolite, optional other Y-type zeolite and optional MFI-structured zeolite, has a rare earth content as rare earth oxide of 10-25 wt% , Eg 11-23 wt%; The unit cell size is 2.440-2.472nm, such as 2.450-2.470nm; Crystallinity is 35-65%, such as 40-60%; The Si / Al atomic ratio of the skeleton is 2.5-5.0; In the X-ray diffraction spectrographic zeolite 2θ = 12.3 ± 0.1 ° peak intensity I 2 2θ = 11.8 ± 0.1 ° the product of the rare earth% by weight as in the rare earth oxide ratio and the zeolite of the peak intensity I 1 at 48 or higher for at, For example, it is 55 or more.
机译:本发明涉及催化裂化催化剂及其制备方法,其中催化裂化催化剂包括催化裂化活性成分,任选的介孔铝硅酸盐材料,粘土和粘合剂,其中催化裂化活性成分是稀有的。包含稀土的Y型沸石包含,由或基本由沸石,任选的其他Y型沸石和任选的MFI结构的沸石组成的含稀土的Y型沸石具有10- 25 wt%,例如11-23 wt%;晶胞尺寸为2.440-2.472nm,例如2.450-2.470nm;结晶度为35-65%,例如40-60%;骨架的Si / Al原子比为2.5-5.0;在X射线衍射光谱中,沸石2θ= 12.3±0.1°峰强度I 2 2θ= 11.8±0.1°稀土氧化物的重量百分比与沸石的乘积峰值强度I 1 在48或更高处的强度,例如,为55或更高。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号