The present invention relates to a method of manufacturing a non-buffing upper material in an adhesion process with improved adhesion strength, and to a non-buffing upper material in an adhesion process produced by this method, and more specifically, to a low-grade split leather without surface treatment. (Split leather) by adjusting the napping properties and applying a fatliquoring agent to solve the problem of adhesion failure, while improving the basic physical properties of abrasion resistance, waterproofness, and fastness, especially in the bonding process, In addition, as the adhesive strength of the adhesive can have properties of 2.0kgf or more, and the buffing process and the primer treatment process are omitted in the bonding process as described above, the conventional 7-step bonding process is used as the 3rd step of the "adhesive application → drying → compression" process. It is possible to shorten it to a step-by-step process (see Fig. 1), which not only allows the shoe manufacturing line to be drastically reduced to within 30m, but also solves the problem of dust and noise in the workplace, easy space for the shoe manufacturing line, and uniform thickness A method of manufacturing a non-buffing upper material in a bonding process with improved adhesion strength, which enables the implementation of process reduction, workplace environment improvement, quality improvement, productivity increase, etc., and a non-buffing upper in the bonding process manufactured by this method It is about the subject matter.
机译:本发明涉及一种在粘合过程中具有改善的粘合强度的非抛光上部材料的制造方法,并且涉及一种通过该方法生产的在粘合过程中的非抛光上部材料,更具体地,涉及一种低等级的不经表面处理的剖层皮革。 (裂皮)通过调节起绒性能并加脂剂来解决粘合失败的问题,同时改善耐磨性,防水性和坚牢度的基本物理性能,特别是在粘合过程中,此外,作为粘合强度的粘合剂可以具有2.0kgf或更高的性能,并且在如上所述的粘合过程中省略了抛光过程和底漆处理过程,常规的7步粘合过程被用作“粘合剂应用→干燥→压缩”过程。可以将其缩短为逐步过程(参见图1),这不仅可以将制鞋生产线大幅减少至30m以内,而且还可以解决工作场所的灰尘和噪音问题,用于制鞋生产线的简单空间和均匀的厚度一种在粘合过程中制造非抛光鞋面材料的方法,具有提高的粘合强度,从而可以减少工艺,改善工作场所环境,提高质量,提高生产率等。通过该方法制造的贴合工序中的非抛光性鞋面和主题。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号