The present invention relates to a method of manufacturing a non-buffing upper material in an adhesion process capable of shortening the adhesion process, and to a non-buffing upper material in the adhesion process manufactured by this method, and more specifically, to a low-grade material without surface processing. By solving the problem of adhesion defects through control of nap and plasma treatment on the split leather of the product, the basic properties such as abrasion resistance, waterproofness, and fastness are improved, while buffing and primer are especially used in the bonding process. The adhesive strength with the shoe sole can have properties of 2.0kgf or more even without a treatment process, and as the buffing process and the primer treatment process are omitted in the bonding process as described above, the conventional 7-step bonding process is "applying adhesive → drying → It is possible to shorten it to a three-step process of the "pressing" process (see Fig. 1), and this allows the shoe manufacturing line to be drastically reduced to within 30m, as well as solving the problem of dust and noise in the workplace, and an easy space for the shoe manufacturing line A method of manufacturing a non-buffing upper material in the bonding process that can shorten the bonding process, which can shorten the process such as securing and realize uniform thickness, improve the workplace environment, improve quality, and increase productivity, and manufactured by this method. It relates to a non-buffing upper material in the gluing process.
机译:本发明涉及一种在能够缩短粘合过程的粘合过程中制造非抛光鞋面材料的方法,并且涉及一种通过这种方法制造的在粘合过程中的非抛光鞋面材料,更具体地,涉及一种高档材料,无需表面处理。通过控制午睡和等离子处理对产品的剖层皮革解决粘合缺陷的问题,改善了诸如耐磨性,防水性和坚牢度之类的基本性能,而粘合过程中特别使用了抛光和底漆。即使不进行处理,与鞋底的粘接强度也可以达到2.0kgf以上。另外,如上所述,由于在结合工序中省略了抛光工序和底漆处理工序,所以以往的7步结合工序为“施加粘合剂→干燥→可以将其缩短为“压制”过程的三步过程(参见图1),这可以将制鞋生产线大幅减少至30m以内,并且可以解决一种在工作场所中的灰尘和噪音的问题,以及用于制鞋生产线的简便空间。一种在粘合过程中制造非抛光鞋面材料的方法,该方法可以缩短粘合过程,从而可以缩短诸如固定并实现均匀的过程。通过这种方法制造的厚度,改善工作环境,提高质量,提高生产率的方法,涉及一种在上胶过程中的非抛光面材料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号