Oxidation Resistance and Critical Sulfur Content of Single-Crystal Superalloys

机译:单晶高温合金的抗氧化性和临界硫含量

获取原文

摘要

The high-temperature components of a jet turbine engine are made from nickel-base superalloys. These components must be able to withstand high stresses, fatigue, and corrosive reactions with high-temperature gases. Such oxidation resistance is associated with slow-growing Al2O3 scales that remain adherent to superalloy components after many thermal cycles. Historically, good oxidation resistance has been obtained by coating these components with Ni-Cr-Al-Y coatings, where small additions of yttrium (Y) were necessary for scale adhesion. Subsequently, it was found that the Y aids scale adhesion by preventing sulfur from segregating to the scale metal interface and thus preventing the sulfur from weakening the oxide-metal bonds. Y is a difficult element to incorporate in single-crystal superalloy castings, but it was shown in early work at the NASA Lewis Research Center that good adhesion could be obtained for low-sulfur, uncoated, singlecrystal superalloys, without Y additions. Low sulfur contents for these uncoated superalloys were achieved in the laboratory by a high-temperature hydrogen annealing process. This process allows segregation and surface cleaning of sulfur monolayers in a reducing environment. Another approach is to remove sulfur from the alloy in the melting process. The present study was designed to establish a guideline for the minimum level of desulfurization needed to achieve maximum performance. Coupons of various thicknesses of the superalloy PWA 1480 were hydrogen annealed at various times (8 to 100 hr) and temperatures (1000 to 1300 C), resulting in coupons with sulfur contents ranging from about 0.05 to 5 ppm. Cyclic oxidation tests at 1100 C were then used to assess adhesion and spalling. The weight change of one set of 20-mil (0.5-mm) samples, annealed for 20 hr at 1000, 1100, 1200, and 1300 C, is shown in the following figure. Clearly, the effect of the annealing temperature is quite dramatic in that the higher temperatures produced scales that spalled very little, whereas the lower temperatures resulted in severe weight losses comparable to those for the as-received, unannealed sample.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号