摘要

Previous evaluations were made to select four high-potential coatings for further testing: ion-vapor-deposited aluminum, sulfamate-nickel electroplate, nickel-cadmium electroplate, and Teflon. Results of six-month field U-bend test exposures in an operating steam turbine are reported. These results generally corroborate the selection of the four high-potential coatings. Fatigue testing at 100 Hz has been initiated in high-purity water and 22% NaCl (both pH 4 solutions). Tests to date generally show a benefit in using one or more of the four candidate coatings. Double U-bend kettle tests are scheduled to start in 1981 in nine test solutions. Test turbine blades have been coated with three of the candidate coatings. These blades will be placed in an operating steam turbine for a one-year test period. (ERA citation 08:045987)

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号