The objective of the work was to investigate temperature impact on corrosion of air-preheater tubes of oil shale CFB boilers. With this objective in view, laboratory corrosion tests of carbon steel St 33 used for manufacturing of air-preheater tubes have been carried out in the atmosphere of air and water steam in the presence of oil shale ash in the temperature range of 75-110 °C. The results have shown that corrosion rate of the metal was maximal at the temperature of 90 °C and minimal at the temperature of 110 °C, which could be recommended as the operation temperature of the metal of air-preheater tubes of oil shale CFB boilers with respect to safe operation of tubes.
机译:该工作的目的是研究温度对油页岩CFB锅炉空气预热管腐蚀的影响。出于这个目的,用于空气预热器管制造的碳钢St 33的实验室腐蚀试验已在空气和水蒸汽的气氛中,在油页岩灰存在的情况下,温度范围为75-110° C。结果表明,金属的腐蚀速率在90°C的温度下最大,在110°C的温度下最小,这可以推荐作为油页岩CFB锅炉空气预热管金属的工作温度。关于管的安全操作。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号