The effect of the granulation and heat treatment of sodium-reduced tantalum powders with a specific surface area of 2.5-3.6 m~2/g on the bulk density, the powder flow time, and the specific surface area of the powders and the specific capacitance of the anodes made of them is studied. It is shown that heat treatment of a granulated powder in vacuum at 1100°C or in a mixture with magnesium at 800°C makes it possible to achieve the required powder flow time.
机译:比表面积为2.5-3.6 m〜2 / g的钠还原钽粉的造粒和热处理对粉体的堆积密度,粉体流动时间,比表面积和比电容的影响研究了由它们制成的阳极。结果表明,在真空中在1100℃下或在与镁的混合物中在800℃下对粒状粉末进行热处理可以实现所需的粉末流动时间。