In this research, a TiO2-activated carbon nano-composite was prepared by a sol-gel method and characterized by XRD, FE-SEM, EDS, FTIR, BET surface area, photoluminescence spectroscopy and UV-Vis diffuse reflectance spectroscopy. The photocatalytic activity of the nano-composite was evaluated through degradation of reactive red 198 (RR 198) under UV light, and was compared to unsupported TiO2. The XRD result indicated that the TiO2 nano-composite contained only anatase phase. The surface area of the TiO2 increased from 48 to 100 m(2)/g through the fabrication of the nano-composite. The photocatalytic results indicated that the RR 198 was decolorized around 42 and 38 % during a 210-min irradiation period in the presence of nano-composite and TiO2, respectively. It means that nano-composite enhanced the photocatalytic activity of the TiO2 nano-particles. After 20 h of irradiation in the presence of the nano-composite, 97 % of RR 198 had degraded.
机译:本研究采用溶胶-凝胶法制备了TiO2活性炭纳米复合材料,并通过XRD,FE-SEM,EDS,FTIR,BET表面积,光致发光光谱和UV-Vis漫反射光谱进行了表征。通过在紫外光下降解活性红198(RR 198)评估了纳米复合材料的光催化活性,并将其与未负载的TiO2进行了比较。 XRD结果表明,TiO2纳米复合材料仅包含锐钛矿相。通过纳米复合材料的制造,TiO2的表面积从48增至100 m(2)/ g。光催化结果表明,在存在纳米复合材料和TiO2的情况下,RR 198在210分钟的照射期间分别脱色了42%和38%。这意味着纳米复合材料增强了TiO2纳米颗粒的光催化活性。在纳米复合材料存在下照射20小时后,RR 198的97%降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号