To investigate the effect of Si/Al ratio, Fe and P loadings on the stability of HZSM-5 in the catalytic cracking of naphtha, experimental tests were done over 20 h time on stream on modified HZSM-5 with different Si/Al molar ratios. NH3-TPD and TPO analyses showed that the more number of weak acid sites, the greater amount of coke is formed. According to TPO and XRD results, it was demonstrated that dealumination had a significant role in catalytic stability. Among catalysts, Fe(6)-P(2)/HZSM-5(25) showed the highest catalytic stability (1.86 wt.% propylene reduction).
机译:为了研究Si / Al比,Fe和P负载量对HZSM-5在石脑油催化裂化中的稳定性的影响,在不同的Si / Al摩尔比的改性HZSM-5上进行了20小时的实验实验。 NH3-TPD和TPO分析表明,弱酸位点数量越多,形成的焦炭量就越大。根据TPO和XRD结果,证明脱铝在催化稳定性中具有重要作用。在催化剂中,Fe(6)-P(2)/ HZSM-5(25)显示出最高的催化稳定性(丙烯还原度为1.86 wt。%)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号