The impact of the addition of CrF3, FeF3, FeF2 and NiF2 to the molten eutectic mixture FLiNaK (46.5 mol% LiF-11.5 mol% NaF-42 mol% KF) on the corrosion behavior of Incoloy 800H/HT was studied by static tests. The mass losses imply that initial corrosion increases upon addition of metal fluorides. Otherwise, the mass losses of alloys in FLiNaK with the same concentration of different additives obey the sequence Cr(3+) < Fe(2+) < Fe(3+) < Ni(2+) which represents the elements' standard electrode potential order. Chromium is acting as a sacrificial element in the cases of addition of FeF2, FeF3 and NiF2 to corrosion media. At the same time chromium and iron act as sacrificial elements in the case of NiF2 addition.
机译:通过静态测试研究了向熔融共熔混合物FLiNaK(46.5 mol%LiF-11.5 mol%NaF-42 mol%KF)中添加CrF3,FeF3,FeF2和NiF2对Incoloy 800H / HT腐蚀行为的影响。质量损失意味着在添加金属氟化物后初始腐蚀增加。否则,在相同浓度的不同添加剂的FLiNaK中合金的质量损失服从Cr(3+)

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号