PREPARATION AND PROPERTIES OF GRAPHITE HEXAFLUOROARSENATES C_xAsF_6 -- PREPARATION OF STAGE-2 C_(28)AsF_6 BY THE REACTION OF STAGE-1 C_(14)ASF_6 WITH GRAPHITE

机译:六氟亚砷酸酯C_xAsF_6的制备和性质-阶段1 C_(14)ASF_6与石墨的反应制备阶段2 C_(28)AsF_6

获取原文
获取原文并翻译 | 示例
           

摘要

Following the reaction of graphite with O_2AsF_6 to produce a stage-1 graphite intercalation compound C_(14)AsF_6, a stage-2 C_(28)AsF_6 was obtained by the reaction of the stage-1 C_(14)AsF_6 with graphite at room temperature, This solid-phase reaction of C_(14)AsF_6 with graphite proceeds relatively fast and the reaction is completed within 24h when an effective mixing is applied to the solid reactants.
机译:石墨与O_2AsF_6反应生成一级石墨插层化合物C_(14)AsF_6后,一级C_(14)AsF_6与石墨在室温下反应获得二级C_(28)AsF_6。在此温度下,C_(14)AsF_6与石墨的固相反应进行得相对较快,当对固体反应物进行有效混合后,该反应会在24小时内完成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号