Northland Resources is developing several magnetite mineral resources in northern Europe. The Tapuli, Sahavaara and Pellivuoma mineral resources are in Sweden and the Hannukainen resource is in Finland. Three of these resources (Sahavaara, Pellivuoma and Hannukainen) require flotation to remove more than 98% by mass of the sulphur in the feedstock to produce a saleable magnetite concentrate with a sulphur level below 0.05% w/w. The detrimental sulphur containing mineral is monoclinic pyrrhotite and its removal requires flotation. Previous published results related to pyrrhotite flotation from magnetite con?centrate, e.g. on a magnetite deposit in Peru, only required the process to produce a final magnetite con?centrate with a sulphur level below 0.4% w/w. There is currently no known published information on a process that floats pyrrhotite to achieve a magnetite concentrate with less than 0.05% w/w of sulphur. Extensive bench-scale tests were conducted on samples from Sahavaara, Pellivuoma and Hannukainen. Low-intensity magnetic separation (LIMS) tests showed that LIMS upgraded the magnetite and the sul?phur in the pyrrhotite at the same ratio.The final flotation reagent regimes and conditions for each deposit were different being related to dif?ferences in mineralogy and grind size. The pH ranged from natural to pH of 4. Large dosage rates of xan-thate collectors and long flotation times were needed. Flotation feed percent solids of between 45% and 50% w/w was required. Future work will modify these reagent regimes and flotation conditions in the full-scale plants to further optimise the flotation processes.
机译:Northland Resources正在北欧开发一些磁铁矿资源。 Tapuli,Sahavaara和Pellivuoma矿产资源位于瑞典,Hannukainen资源位于芬兰。这些资源中的三种(Sahavaara,Pellivuoma和Hannukainen)需要浮选以去除原料中98%质量以上的硫,以生产硫含量低于0.05%w / w的可销售磁铁矿精矿。有害的含硫矿物是单斜黄铁矿,其去除需要浮选。以前发表的结果与磁铁矿精矿中黄铁矿浮选有关。在秘鲁的磁铁矿矿床中,只需要生产硫含量低于0.4%w / w的最终磁铁矿精矿的过程即可。目前尚无关于使磁黄铁矿浮选以得到硫含量小于0.05%w / w的磁铁矿精矿的方法的公开信息。对来自Sahavaara,Pellivuoma和Hannukainen的样本进行了广泛的基准测试。低强度磁选(LIMS)试验表明,LIMS以相同的比例提质了黄铁矿中的磁铁矿和硫磺。每种矿床的最终浮选剂制度和条件都不同,这与矿物学和研磨的差异有关尺寸。 pH值范围从自然到pH为4。需要使用大剂量的黄原酸酯捕收剂,并且浮选时间较长。需要浮选进料固体百分比为45%至50%w / w。未来的工作将修改大规模工厂中的这些试剂方案和浮选条件,以进一步优化浮选过程。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号