Intensification of Sulfide Copper-Nickel Ore Heap Leaching with Bioreagent-Oxidant Participation

机译:生物试剂-氧化剂参与强化硫化铜镍矿堆浸

获取原文
获取原文并翻译 | 示例

摘要

With the aim of intensification, improving economic efficiency, and controlling sulfide ore heap bacterial leaching features and leaching regimes are studied for lean copper-nickel ore with the participation of a bioreagent-oxidant prepared by iron-oxidizing micro-organisms and concentrated adsorption immobilization in a separate reactor. Research established the ore size for heap leaching and an increase in metal extraction with an increase in bioreagent concentration. Use of the heap bioleaching technology developed for ore with a size of -10 mm containing 0.32% nickel and 0.11% copper makes it possible to increase nickel extraction into solution to 6.3-19.5% and copper to 5.8-24.2% with consumption of sulfuric acid lower by 4.4-14.6% compared with use of seeding ore with bacteria.
机译:以集约化,提高经济效益,控制硫化物矿石堆为研究对象,研究了铁-氧化微生物和浓缩吸附固定化制备的生物试剂-氧化剂参与的贫铜-镍矿的细菌浸出特性和浸出方式。一个单独的反应堆。研究确定了堆浸的矿石大小,并随着生物试剂浓度的增加而增加了金属提取量。使用为-10毫米尺寸的矿石(含0.32%的镍和0.11%的铜)开发的堆浸生物浸出技术,可以通过消耗硫酸将镍的溶解度提高到6.3-19.5%,将铜的萃取率提高到5.8-24.2%与使用细菌播种矿石相比,降低了4.4-14.6%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号