Effect of the duration of austempering on particle erosion wear resistance of ADI was studied. In short duration (Stage I) region, a fair amount of martensite phase can be recognized, and hence deterioration of erosion wear resistance. In initial Stage II, the austempering region (0.5 hr duration) is free of carbide. If prolonged the austempering duration, the retained austenite amount tend to decrease and hence carbide formation. Even if slightly increase of carbide amount that still can play an important role on debasing wear resistance, resulted from the alternation of erosion behavior. Erosion-induced phase transformation of retained austenite also can be determined that is generality transformed to e-carbide.
机译:研究了奥氏体回火时间对ADI抗颗粒侵蚀磨损性能的影响。在短时间(阶段I)区域中,可以识别出大量的马氏体相,因此耐侵蚀磨损性变差。在初始阶段II,奥氏体回火区(0.5小时持续时间)不含碳化物。如果延长奥氏体化时间,则残留奥氏体量趋于减少,从而形成碳化物。即使碳化物的量略有增加,仍然可以在降低耐磨损性方面发挥重要作用,这是由腐蚀行为的交替引起的。还可以确定由腐蚀引起的残余奥氏体的相变,该相变通常被转化为e-碳化物。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号