The erosion corrosion failure of elbow of one oil refinery was investigated by using Aspen software, CFD technology and experiments. And the gas-liquid equilibrium distribution of H2S and NH3 and multiphase flow simulation in the overhead system of a sour water stripper were obtained. The result shows that the component mole fraction of H2S and NH3 rises markedly with decreasing temperature. At the outlet of air cooler, the temperature drops to 85 degrees C to form high concentration of ammonium bisulfide (NH4HS), which would cause serious erosion corrosion at a certain flow rate and reveals an inhomogeneous thinning. The liquid phase fraction mainly distributes on the outside part of elbow, the more sour water accumulates there resulting in localized corrosion thinning. Meanwhile, the experiments show that when the concentration of NH4HS reaches 10 wt.%, the corrosion rates increase rapidly with increased velocity. Thus controlling the concentration of NH4HS below 10 wt.% in reflux drum would reduce the risk of erosion corrosion failure. (C) 2016 Elsevier Ltd. All rights reserved.
机译:利用Aspen软件,CFD技术和实验研究了某炼油厂弯头的腐蚀腐蚀破坏。并获得了酸式汽提塔塔顶系统中H2S和NH3的气液平衡分布以及多相流模拟。结果表明,H 2 S和NH 3的组分摩尔分数随温度降低而显着增加。在空气冷却器的出口,温度下降到85摄氏度,形成高浓度的二硫化铵(NH4HS),这将在一定流速下引起严重的腐蚀腐蚀,并显示出不均匀的稀化。液相部分主要分布在弯头的外部,酸性水积聚在弯头的外部,导致局部腐蚀变稀。同时,实验表明,当NH4HS的浓度达到10 wt。%时,腐蚀速率随速度的增加而迅速增加。因此,将回流罐中的NH4HS浓度控制在10 wt。%以下将减少侵蚀腐蚀失效的风险。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号